2-乙基己酸甲酯 Methyl 2-Ethylhexanoate 816-19-3
2-乙基-己酸稀土盐 2-Ethylhexanoic Acid 149-57-5合成工艺路线路线简述
- 合成目标产物 Triethylene Glycol Bis(2-Ethylhexanoate) 主要起始原料 2-Ethylhexanoic Acid And Triethylene Glycol
- 149-57-5 + 112-27-6 = 94-28-0
反应条件:1.1 Catalysts: Stannous Octoate; Rt -> 240 °C; 3.5 H,225 - 240 °C
标题:Green Preparation Of Stannous Isooctenoate As Catalyst In Polyester Reaction
参考文献:China]
149-57-5 + 112-27-6 = 94-28-0
反应条件:1.1 Rt -> 80 °C; 2 H,40 - 80 °C; 6 H,80 - 90 °C; 90 °C -> Rt1.2 Reagents: Sodium Hydroxide Solvents: Water; 1 H,Rt
标题:Preparation Method Of Triethylene Glycol Diisooctanoate
参考文献:China]
149-57-5 + 112-27-6 = 94-28-0
反应条件:1.1 Catalysts: Titanium Tetrachloride,Barium Sulfate; 10 H,160 °C
标题:Synthetic Process Of Triethylene Glycol Diisooctanate
参考文献:China]
149-57-5 + 112-27-6 = 94-28-0
反应条件:1.1 Reagents: Carbon Catalysts: Stannous Chloride,Titania; 50 Kpa,Rt -> 85 °C; 4 H,85 °C
标题:Production Method Of Triethylene Glycol Di-2-Ethylhexoate
参考文献:China]
149-57-5 + 112-27-6 = 94-28-0
反应条件:1.1 Catalysts: Titanium Isopropoxide,Zirconium Phosphate (Zr(Hpo4)2) Solvents: Dimethylformamide; Rt -> 205 °C; 10 H,205 °C
标题:A Method For Preparing Plasticizer Triethylene Glycol Bis(2-Ethylhexanoate)
参考文献:China]
149-57-5 + 112-27-6 = 94-28-0
反应条件:1.1 Catalysts: Titanium Isopropoxide; 0.6 Bar,Rt -> 220 °C; 1 H,0.4 Bar,220 °C; 3 H,0.3 Bar,220 °C
标题:Production Of Polyol Esters By Reacting Polyols With Aliphatic Carboxylic Acids In Presence Of Lewis Acid And Adsorbers
参考文献:Germany]
149-57-5 + 112-27-6 = 94-28-0
反应条件:1.1 Reagents: Carbon; 900 Hpa,Rt -> 225 °C; 900 Hpa -> 400 Hpa,225 °C; 14 H,400 Hpa,5 °C1.2 Reagents: Potassium Hydroxide
标题:Method For Manufacturing Of Polyol Esters Using Partial Recycling Of The Aliphatic Monocarboxylic Acids
参考文献:European Patent Organization]
149-57-5 + 63468-14-4 = 94-28-0
反应条件:1.1 Catalysts: Zirconium Dioxide (Sulfated),Hnd 32; 463.15 - 493.15 K
标题:A Novel Process For The Production Of Triethylene Glycol Di-2-Ethylhexoate By Reactive Distillation Using A Sulfated Zirconia Catalyst
作者:Li,Xingang; Zhang,Qingyu; Li,Hong; Gao,Xin
参考文献:Industrial & Engineering Chemistry Research 日期:2020 卷标:59(19) 页码:9242-9253]
149-57-5 + 112-27-6 = 94-28-0
反应条件:1.1 Solvents: Water; 8 H,120 °C
标题:Synthesis Method For Triethylene Glycol Diisooctanoate
参考文献:China]
149-57-5 + 112-27-6 = 94-28-0
反应条件:1.1 12 - 16 H,0.01 - 0.02 Kpa,180 - 220 °C
标题:Esterification And Deacidification Two-In-One Device For Production Of Triethylene Glycol Di-Isooctanoate
参考文献:China]
149-57-5 + 112-27-6 = 94-28-0
反应条件:1.1 Catalysts: Titanium Isopropoxide; Rt -> 205 °C; 0.5 H,0.7 Bar,205 °C; 205 °C -> 210 °C; 1.5 H,0.6 Bar,210 °C; 0.4 Bar,210 °C -> 215 °C; 5 H,0.15 Bar,215 °C; 0.5 H,215 °C; 6 H,0.05 Bar,215 °C; Cooled1.2 Reagents: Sodium Metasilicate (Na2Sio3),Hydrogen Peroxide; Rt -> 105 °C; 1 H,105 °C
标题:Preparing Glycol Esters With Low Color And Peroxide Content
参考文献:World Intellectual Property Organization]
149-57-5 + 112-27-6 = 94-28-0
反应条件:1.1 Reagents: Sodium Hypophosphite Solvents: Xylene; 450 Min,235 °C1.2 Reagents: Sodium Hydroxide Solvents: Water; Neutralized
标题:Method For Producing An Ester By Reacting Diol With Monocarboxylic Acid In Presence Of Azeotropic Solvent And Antioxidant
参考文献:Sweden]
149-57-5 + 112-27-6 = 94-28-0
反应条件:1.1 60 °C; 3 H,0.05 - 0.2 Mpa,210 - 220 °C; 1 - 1.5 H,0.01 - 0.02 Mpa,220 - 225 °C
标题:Preparation Method Of Environment-Friendly Plasticizer Triethylene Glycol Bis(2-Ethylhexanoate)
参考文献:China]
149-57-5 + 112-27-6 = 94-28-0
反应条件:1.1 Catalysts: Titanium Isopropoxide
标题:Process For Preparing Polyol Ester-Enriched Product Streams From Side Streams In Polyol Ester Production
参考文献:Germany]
149-57-5 + 112-27-6 = 94-28-0
反应条件:1.1 200 - 250 °C
标题:Polyglycerin-Based Plasticizers And Thermoplastic Resin Compositions Containing Them
参考文献:World Intellectual Property Organization]
149-57-5 + 112-27-6 = 94-28-0
反应条件:1.1 Catalysts: Phosphinic Acid,Butyltin Oxide Solvents: Water; 150 - 200 °C; 7 H,200 °C -> 220 °C1.2 Reagents: Sodium Hydroxide Solvents: Water
标题:Method For Preparation Of Ester Plasticizer With High Purity And Low Hue
参考文献:China]
149-57-5 + 112-27-6 = 94-28-0
反应条件:1.1 Reagents: Carbon; 900 Hpa,Rt -> 225 °C; 900 Hpa -> 400 Hpa,225 °C; 14 H,400 Hpa,5 °C1.2 Reagents: Potassium Hydroxide
标题:Method For Brightening The Color Of Polyol Esters Using Ozone Treatment
参考文献:European Patent Organization]
149-57-5 + 112-27-6 = 94-28-0
反应条件:1.1 Reagents: Carbon; 900 Hpa,Rt -> 225 °C; 900 Hpa -> 400 Hpa,225 °C; 14 H,400 Hpa,5 °C1.2 Reagents: Potassium Hydroxide
标题:Method For Brightening The Color Of Polyol Esters
参考文献:European Patent Organization
2-乙基己酰氯置于potassium Carbonate体系中,用 丙醇 作为反应溶剂,化学反应 4.0H,反应生成 三乙二醇二异辛酸酯
参考文献: Synthesis Of Triethylene Glycol Bis(2-Ethylhexanoate)[fr] Synthèse De Triéthylène Glycol Bis(2-éthylhexanoate)
标题: Synthesis Of Triethylene Glycol Bis(2-Ethylhexanoate)[fr] Synthèse De Triéthylène Glycol Bis(2-éthylhexanoate)
摘要:提供了一种用三乙二醇对甲基-2-乙基己酸酯进行酯交换反应以产生三乙二醇二-2-乙基己酸酯的方法.在该过程中,将甲基-2-乙基己酸酯与三乙二醇混合形成第一混合物.在催化剂的存在下加热第一混合物,形成包含甲醇和三乙二醇二-2-乙基己酸酯的第二混合物.将甲醇从第二混合物中分离出来,得到三乙二醇二-2-乙基己酸酯.na2Co3,Cs2Co3,K2Co3,Rb2Co3,甲基钠或异丙酸钛是适合的催化剂.
海关参考信息
- 2905121000-正丙醇
2905310000-1,2-乙二醇
2909110000-乙醚
2912110000-甲醛 - 💡 提示:海关信息按照顺序优先匹配,如需确认的海关信息,请参考相关资料。
- 详情请参考:📖 海关编码查询和海关进出口税则
专利信息
专利号:US-10829429-B2
优先权日:2018-11-13
标 题:Synthesis of triethylene glycol bis(2-ethylhexanoate)
发明人:CHAKRABORTY SUMIT; ADAMS STEVEN J; HEMBRE ROBERT THOMAS; BARNICKI SCOTT DONALD; JENKINS DAVID ALAN
权利人:EASTMAN CHEM CO
摘要:A process for the transesterification of methyl-2-ethylhexanoate with triethylene glycol to produce triethylene glycol di-2-ethylhexanoate is provided. In the process, methyl-2-ethylhexanoate is combined with triethylene glycol to form a first mixture. The first mixture is heated in the presence of a catalyst to form a second mixture comprising methanol and triethylene glycol di-2-ethylhexanoate. Methanol is separated from the second mixture to yield triethylene glycol di-2-ethylhexanoate. Na2CO3, Cs2CO3, K2CO3, Rb2CO3, sodium methoxide or titanium isopropoxide are suitable catalysts.
专利号:US-2020148619-A1
优先权日:2018-11-13
标题 :Synthesis of triethylene glycol bis(2-ethylhexanoate)
专利号:US-5194469-A
优先权日:1991-02-28
标题:Latex for coatings having improved flexibility
发明人:SRAIL RICHARD E; BURROWAY GARY L
权利人:GOODYEAR TIRE & RUBBER
摘要:This invention relates to the synthesis of a latex which can be formulated into coatings having improved flexibility and good water resistance. Coatings of this type are particularly useful in roof coating applications because they offer excellent flexibility, excellent ultra-violet light resistance, and good water resistance. The subject invention more specifically discloses a process for producing a neutralized latex that is useful in the manufacture of water reducible coatings which comprises: n (1) free radical aqueous emulsion polymerizing, at a pH of less than about 3.5, a monomer mixture which comprises, based on 100 weight percent monomers: (a) from about 30 to about 70 weight percent vinyl aromatic monomers, (b) from about 25 to about 65 weight percent of at least one alkyl acrylate monomer, (c) from about 1 to about 5 weight percent of acrylic acid, and (d) about 0.4 to about 3 weight percent methacrylic acid, in the presence of about 0.2 to 0.4 phm at least one sulfonate surfactant and in the presence of about 4 to 8 phm of at least one nonionic surface active agent having a hydrophile-lipophile balance number which is within the range of about 12 to about 20 to produce a latex; and n (2) neutralizing the latex with ammonia to a pH which is within the range of about 7 to about 10.5 to produce the neutralized latex.
专利号:US-5122566-A
优先权日:1989-10-06
标 题 :Latex for coatings having reduced blushing characteristics
发明人:BURROWAY GARY L; GESENHUES ALBERT M; BRADEN JENNIFER T
权利人:GOODYEAR TIRE & RUBBER
摘要:This invention relates to the synthesis of a latex which can be formulated into coatings having improved water resistance for both moisture vapor transmission and water spotting. Coatings which are formulated with the latex of this invention are particularly useful for coating metal substrates because they provide excellent rust and corrosion resistance. The subject invention more specifically discloses a process for producing a neutralized latex that is useful in the manufacture of water reducible coatings which comprises: (1) free radical aqueous emulsion polymerizing at a pH of less than about 3.5 a monomer mixture which comprises, based on 100 weight percent monomers: (a) from about 45 to about 85 weight percent vinyl aromatic monomers, (b) from about 15 to about 50 weight percent of at least one alkyl acrylate monomer, and (c) from about 1 to about 6 weight percent of at least one unsaturated carbonyl compound; in the presence of about 0.5 to 4.0 phm at least one phosphate ester surfactant and in the presence of about 0.5 to 4.0 phm of at least one water insoluble nonionic surface active agent to produce a latex; and (2) neutralizing the latex with ammonia to a pH which is within the range of about 7 to a bout 10.5 to produce the neutralized latex.
专利号:WO-2020102128-A1
优先权日:2018-11-13
标 题:Synthesis of triethylene glycol bis(2-ethylhexanoate)
专利号:US-4968741-A
优先权日:1989-10-06
标题:Latex for coatings having reduced blushing characteristics
发明人:BURROWAY GARY L; GESENHUES ALBERT M; BRADEN JENNIFER T
权利人:GOODYEAR TIRE & RUBBER
摘要:This invention relates to the synthesis of a latex which can be formulated into coatings having improved water resistance for both moisture vapor transmission and water spotting. Coatings which are formulated with the latex of this invention are particularly useful for coating metal substrates because they provide excellent rust and corrosion resistance. The subject invention more specifically discloses a process for producing a neutralized latex that is useful in the manufacture of water reducible coatings which comprises: n (1) free radical aqueous emulsion polymerizing at a pH of less than about 3.5 a monomer mixture which comprises, based on 100 weight percent monomers: (a) from about 45 to about 85 weight percent vinyl aromatic monomers, (b) from about 15 to about 50 weight percent of at least one alkyl acrylate monomer, and (c) from about 1 to about 6 weight percent of at least one unsaturated carbonyl compound; in the presence of about 0.5 to 4.0 phm at least one phosphate ester surfactant and in the presence of about 0.5 to 4.0 phm of at least one water insoluble nonionic surface active agent to produce a latex; and n (2) neutralizing the latex with ammonia to a pH which is within the range of about 7 to about 10.5 to produce the neutralized latex.